MES, Inc.
Technology & Transformation
NOVEMBER 2026
5 min read

Die Casting for Electrical Enclosures and Switchgear: Draft, Wall Thickness, and What Tolerance Actually Costs

Summary

Most engineers who specify die cast enclosures were never taught to design for the process. Draft angle, uniform wall thickness, parting line placement and rib design all have rules that affect cost and quality more than any material choice does — and tolerance is where an unexamined callout adds a machining operation to every part for the life of the program.

KEY TAKEAWAYS

Thick sections do not add strength. Molten metal solidifies from the wall inward, so a heavy section is the last place to freeze and the place where shrinkage porosity collects. Stiffness comes from ribs and geometry, not from mass.
Tolerance is a step function, not a slope. There is a grade achievable as-cast and a grade requiring a secondary machining operation, and the boundary between them is invisible on a drawing. One grade tighter than necessary adds an operation to every part, forever.
Draft is not optional and it is not uniform. Two degrees is a reasonable default on an external wall, but a deep pocket, a textured surface or a long core all need more — and a drawing showing zero draft is a drawing that cannot be made.

ARTICLE

An enclosure drawing arrives with square corners, a wall stepping from 3 mm to 9 mm around a mounting boss, no draft called out, and a tolerance block applied uniformly. It gets quoted high, and first articles come back with porosity in the thick section and dimensions needing a secondary operation nobody budgeted for.

None of that is the caster’s doing. It is the predictable outcome of a part designed as though it would be machined from solid stock.

Draft: the angle that lets the part leave the die

A die cast part has to eject from a steel cavity, and any surface parallel to the ejection direction drags on the way out. Two degrees is a reasonable default on an external aluminum wall. More is needed on deep pockets and long cores, on textured surfaces where the texture is itself an undercut, and on inside walls, which shrink onto the core rather than away from the cavity. Less is possible on short polished walls, down to about half a degree.

What is not possible is zero. A drawing showing a vertical wall with no draft gets quoted with draft added by the caster, changing the geometry, or machined afterward — both decisions made by someone other than the designer.

Wall thickness: uniform, and thinner than you think

Molten aluminum solidifies from the die wall inward. A thin section freezes evenly; a thick one freezes from the outside first, and the metal in the center is still liquid when the shell around it has contracted — so the last metal to solidify has nowhere to draw from, and shrinkage porosity forms in the heaviest part of the section.

So the thick boss added for strength is frequently weaker than the wall beside it, and the porosity is invisible until a cut opens it or a load finds it.

For A380: 2 to 3 mm is a comfortable nominal wall, 1.5 mm is achievable on a good flow path, and above about 5 mm should be justified. Where sections change, transition over a generous radius — a 3 mm wall meeting a 6 mm boss with a sharp step is a hot spot.

Stiffness comes from ribs. A 2.5 mm wall with ribs at roughly 60 percent of the wall thickness is stiffer, lighter, cheaper and sounder than a 5 mm wall with none.

Parting line and ribs

The parting line is where the die halves meet and it leaves a witness on the part. It also determines what geometry is possible without a slide, because anything undercut relative to the draw needs one — and every slide is tooling cost, cycle time and a flash location.

Put it where a witness mark is acceptable rather than where it is convenient, and keep critical dimensions within one die half — a dimension spanning the parting line carries die closure tolerance on top of everything else.

Ribs go thinner than the wall they support, radiused at the base, drafted like everything else. A rib thicker than its wall creates the same hot spot as any heavy section.

Thermal Cycling: The Slow Way Insulation Fails

This is the commercially useful half, and it is a step function rather than a slope.

Requirement How it is achieved Cost effect
Standard as-cast tolerance Straight from the die Baseline
Precision as-cast Tighter tool, tighter process control Modest premium
Beyond as-cast capability Secondary machining operation Step change. New setup, new fixture, per part
Tight tolerance across the parting line Machining, or a redesign Highest. Die closure adds to the stack

The step is what matters. Within as-cast capability, tightening costs process control and inspection. Past it, the part acquires a machining operation — a second setup, a fixture, and a per-part cost for the life of the program.

And the drawing gives no indication. A dimension one grade tighter than necessary looks identical on paper, and the cost does not appear until the quote — by which point changing it is a revision.

Which argues for reviewing tolerances individually rather than applying a block. The dimensions genuinely needing tight control are mounting interfaces, sealing surfaces and bearing bores — frequently machined anyway. A uniform tolerance across the part means paying for the tightest one everywhere.

Frequently Asked Questions

What draft angle is required for die casting?

A die cast part has to eject from a steel cavity, and any surface parallel to the ejection direction drags as it comes out. Two degrees is a reasonable default on an external aluminum wall. More is needed on deep pockets and long cores, on textured surfaces, and on inside walls that shrink onto the core as the part cools. Less is possible on short polished walls in the ejection direction, down to about half a degree. Zero draft is not achievable — a drawing showing it will be quoted with draft added or with a machining operation.

Because molten aluminum solidifies from the die wall inward. A thick section freezes from the outside first, and the metal in the center is still liquid when the surrounding shell has contracted around it — so the last metal to solidify has nowhere to draw from and shrinkage porosity forms in the heaviest part of the section. The thick boss added for strength is frequently weaker than the thin wall beside it.

In A380, 2 to 3 millimeters is a comfortable nominal wall, and 1.5 millimeters is achievable on a well-designed flow path. Anything above about 5 millimeters should be justified rather than assumed. Where sections change, transition gradually over a generous radius rather than a sharp step, which creates a hot spot.

Ribs. A 2.5 millimeter wall with well-placed ribs at roughly 60 percent of the wall thickness is stiffer, lighter, cheaper and sounder than a 5 millimeter wall with none. Ribs should be thinner than the wall they support, generously radiused at the base and drafted like every other surface — a rib thicker than its wall creates the same hot spot as any heavy section.

When it exceeds what the process holds as-cast. Within as-cast capability, tightening costs process control and inspection. Past it, the part acquires a machining operation with a second setup, a fixture and a per-part cost that runs for the life of the program — and the drawing gives no indication that it happened.

MES die casts enclosures, mechanism housings and structural hardware in aluminum and zinc across eight countries, with gating reviewed before the tool is cut rather than after the first return. On a cast enclosure that review usually finds a thick section added for strength and a tolerance block applied where three dimensions needed it.

Talk to us about a casting on your drawing